First results on the phase 1 demonstration are looking promising. Zinc is recovered from non-ferrous flows derived form bottom ashes using sensor sorting technology. The innovative part regarding this sensor sorting is that we are separating relative fine zinc particles (0-12mm) from bottom aches into a zinc concentrate which is suitable for the Elemetal leaching process. Using these sensor sort technologies, the project is able to recover up to 70% of the zinc currently present in bottom ashes. 

This zinc is leached and converted into zinc sulpate solution at a recovery rate of >95% which is sold to different industries.